(12) Patent Application Publication (10) Pub. No.: US 2006/ A1

Size: px
Start display at page:

Download "(12) Patent Application Publication (10) Pub. No.: US 2006/ A1"

Transcription

1 (19) United States US A1 (12) Patent Application Publication (10) Pub. No.: US 2006/ A1 Sumrall (43) Pub. Date: (54) LIGHTWEIGHT CONCRETE COMPOSITE of application No. 09/887,369, filed on Jun. 22, 2001, BLOCKS now Pat. No. 6,827,570. (75) Inventor: Orbin F. Sumrall, San Antonio, TX (60) Provisional application No. 60/605,102, filed on Aug. (US) 27, Correspondence Address: Publication Classification LAW OFFICES OF CHRISTOPHER L. MAKAY (51) Int. Cl Milam Building E04C I/00 ( ) 115 East Travis Street (52) U.S. Cl / San Antonio, TX (US) (73) Assignee: AMAZON FORMS ONE, INC. (57) ABSTRACT (21) No.: Appl. No 11/209, , A lightweight gnlwelg concrete composite p is utilized to form blocks. The lightweight concrete composite includes polystyrene, (22) Filed: Aug. 22, 2005 cement, water, and glass. The blocks are advantageous for building retaining structures in the form of walls, enclosed Related U.S. Application Data areas, raised gardens, flower beds, and the like because the blocks are lightweight, easily cut and Stacked, and more (63) Continuation-in-part of application No. 10/374,886, importantly do not introduce harmful chemicals into the filed on Feb. 26, 2003, which is a continuation-in-part environment.

2 Patent Application Publication US 2006/ A1

3 LIGHTWEIGHT CONCRETE COMPOSITE BLOCKS CROSS-REFERENCE TO RELATED APPLICATIONS This application is a continuation-in-part of appli cation Ser. No. 10/374,886, filed Feb. 26, 2003, which was a continuation-in-part of U.S. Pat. No. 6,827,570 B2, issued Dec. 7, This present application claims all available ben efit, under 35 U.S.C. S 119(e), of U.S. provisional patent application Ser. No. 60/605,102, filed Aug. 27, By this reference, the full disclosure of U.S. provisional patent application Ser. No. 60/605,102 is incorporated herein as though now Set forth in its entirety. BACKGROUND OF THE INVENTION 0003) 1. Field of the Invention The present invention relates to lightweight con crete and, more particularly, but not by way of limitation, to unitary lightweight concrete composite blocks Description of the Related Art 0006 Landscaping as well as gardening often requires the building of retaining Structures in the form of walls, enclosed areas, and raised gardens or flower beds. Hereto fore, landscape timbers have been the primary materials used in the construction of Such walls, enclosed areas, and raised gardens or flower beds. While landscape timbers have functioned adequately, there are certain disadvantages in their use. Landscape timbers are chemically treated to make them resistant to rot and decay. Unfortunately, the chemicals employed to treat the landscape timbers, in particular arsenic and creosote, are toxic and thus harmful to the environment. Consequently, pollution occurs not only at production facili ties but also at points of use Since landscape timbers leach the treatment chemicals into the Surrounding environment. Furthermore, landscape timbers ultimately rot and decay necessitating replacement in addition to more fully deliver ing the treatment chemicals into the environment. Accord ingly, a block Suitable for use in constructing walls, enclosed areas, and raised gardens or flower beds that is not chemi cally treated as well as resistant to rot and decay would be a significant improvement over current landscape timbers. SUMMARY OF THE INVENTION In accordance with the present invention, a light weight concrete composite block includes polystyrene, cement, water, and glass mixed to formulate a lightweight concrete composite, which is then cured into the lightweight concrete composite block. The polystyrene may be recycled polystyrene ground into particles having a diameter of less than of an inch. The polystyrene comprises between 75% and 95% by total volume of the cement. The glass may be recycled glass ground into particles having a diameter of less than 4 of an inch. The glass comprises between 40% and 45% by total weight of the cement. The water comprises between 40% and 50% by total weight of the cement. The lightweight concrete composite block may also include fly ash Substituted for cement up to 20% by total weight of the cement. The lightweight concrete composite block may further include a calcium chloride accelerator mixed with the polystyrene, cement, water, and glass in an amount equal to 2% of total weight of the cement. The lightweight concrete composite block may still further include a hard ening agent mixed with the polystyrene, cement, water, and glass in an amount equal to 2% of total weight of the cement In accordance with the present invention a method of manufacturing lightweight concrete composite blocks includes mixing polystyrene, cement, water, and glass to formulate a lightweight concrete composite and curing the lightweight concrete composite into lightweight concrete composite blocks. The polystyrene is ground into particles having a diameter of less than of an inch prior to mixing the polystyrene with the cement, water, and glass to formulate the lightweight concrete composite. The polystyrene com prises between 75% and 95% by total volume of the cement. The glass is ground into particles having a diameter of less than /4 of an inch prior to mixing the glass with the polystyrene, cement, and water to formulate the lightweight concrete composite. The glass comprises between 40% and 45% by total weight of the cement. The water comprises between 40% and 50% by total weight of the cement. The lightweight concrete composite block may also include fly ash substituted for cement up to 20% by total weight of the cement. The lightweight concrete composite block may further include a calcium chloride accelerator mixed with the polystyrene, cement, water, and glass in an amount equal to 2% of total weight of the cement. The lightweight concrete composite block may still further include a hard ening agent mixed With the polystyrene, cement, Water, and glass in an amount equal to 2% of total weight of the cement In accordance with the present invention, a method of installing lightweight concrete composite blocks to build a retaining Structure includes the use of lightweight concrete composite blocks comprising polystyrene, cement, water, and glass mixed to formulate a lightweight concrete com posite, which is then cured into the lightweight concrete composite blocks. A first lightweight concrete composite block is cut to a desired length and placed at a desired location. A Second lightweight concrete composite block is cut to a desired length, placed on the first lightweight concrete composite block, and then Secured with the first lightweight concrete composite block. A third lightweight concrete composite block is cut to a desired length, placed adjacent the first lightweight concrete composite block, and Secured with the first lightweight concrete composite block. A fourth lightweight concrete composite block is cut to a desired length, placed on the third lightweight concrete composite block and adjacent the Second lightweight con crete composite block, and Secured with the Second and third lightweight concrete composite blocks It is therefore an object of the present invention to provide lightweight concrete composite blocks comprised of polystyrene, cement, Water, and glass It is another object of the present invention to provide lightweight concrete composite blocks that do not introduce harmful chemicals into the environment It is a further object of the present invention to provide a method of manufacturing lightweight concrete composite blocks comprised of polystyrene, cement, water, and glass It is still a further object of the present invention to provide lightweight concrete composite blocks Suitable for the building of retaining Structures.

4 0.014 Still other objects, features, and advantages of the present invention will become evident to those of ordinary skill in the art in light of the following. BRIEF DESCRIPTION OF THE DRAWINGS FIG. 1 is a perspective view illustrating a unitary lightweight concrete block according to a preferred embodi ment FIG. 2 is a perspective view illustrating the use of unitary lightweight concrete blocks according to a preferred embodiment for building a retaining structure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENT As illustrated in FIGS. 1 and 2, a unitary light weight concrete composite block 10 is rectangular with a horizontal axis greater than a vertical axis to facilitate Stacking thereof for the building of retaining Structures in the form of walls, enclosed areas, raised gardens, flower beds, and the like. While the preferred embodiment of the block10 is rectangular to facilitate easier Stacking thereof, those of ordinary skill in the art will recognize many alternative shapes, including but not limited to Square, circular, trian gular, polygonal, L-shaped, and the like The lightweight concrete composite utilized to form the blocks 10 includes polystyrene, which is typically recycled; cement, which is typically Portland; water, and glass, which is typically recycled, ground glass. The cement is Stored in a hopper prior to delivery from the hopper into a mixer using Suitable and well-known means Such as an auger, conveyor belt, pneumatic blower, and the like. Like wise, the water is Stored in a tank prior to delivery from the tank into the mixer using Suitable and well-known means Such as a pump, gravity feed, and the like. The polystyrene is loaded into a grinder, which is of a type well known to those of ordinary skill in the art, and ground into particles having a diameter of less than of an inch. After grinding, the polystyrene particles are Stored in a hopper prior to delivery from the hopper into the mixer using Suitable and well known means Such as an auger, conveyor belt, pneumatic blower, and the like. Likewise, the glass is loaded into a grinder, which is of a type well known to those of ordinary skill in the art, and ground into particles having a diameter of less than /4 of an inch. After grinding, the glass particles are Stored in a hopper prior to delivery from the hopper into the mixer using Suitable and well-known means Such as an auger, conveyor belt, and the like Lightweight concrete composite utilized in manu facturing blocks 10 is formulated by delivering the cement, water, polystyrene particles, and glass particles into the mixer. Cement is delivered into the mixer in a desired amount. Water is delivered into the mixer in an amount between 40% and 50% by total weight of the cement. Polystyrene particles are delivered into the mixer in an amount between 75% and 95% by total volume of the cement. Glass particles are delivered into the mixer in an amount between 40% and 45% by total weight of the cement. The mixer, which is of a type well known to those of ordinary skill in the art, combines the cement, water, polystyrene particles, and glass particles, thus forming a lightweight concrete composite After formulation of the lightweight concrete com posite, the mixer delivers the lightweight concrete compos ite into forms via a Screed assembly Such as that disclosed in U.S. patent application Ser. No. 10/374,886, the disclo sure of which is herein incorporated by reference. The forms are identical to the forms disclosed in U.S. patent application Ser. No. 10/374,886, except the cap is unnecessary and thus eliminated and the bottom assemblies are Segmented to provide individual molds that produce multiple blocks 10. The mixer delivers the lightweight concrete composite into the Screed assembly, which, in turn, delivers the lightweight concrete composite into a form. Once the Screed assembly completes delivery of the lightweight concrete composite into the form, a curing oven, Such as that disclosed in U.S. patent application Ser. No. 10/374,886, cures the lightweight concrete composite within the form. A block removal Sta tion, Such as that disclosed in U.S. patent application Ser. No. 10/374,886, removes the cured lightweight concrete composite blocks 10 from the form. A conveying System, Such as that disclosed in U.S. patent application Ser. No. 10/374,886, routes forms in a continuous loop simulta neously through the Screed assembly, curing oven, and block removal Station, thereby creating a time efficient process The lightweight concrete composite utilized to form the blocks 10 includes at least polystyrene, cement, water and glass, however, the cost of formulating the light weight concrete composite may be reduced through the substitution of fly ash for a portion of the cement. In particular, fly ash may be Substituted for cement up to 20% by total weight of the cement. Consequently, fly ash may be added to any formulation up to 20% by total weight of the cement Furthermore, due to varying atmospheric condi tions, in particular, temperature and humidity, it may be necessary to include in the lightweight concrete composite other additives that improve the performance characteristics thereof. One Such additive is a calcium chloride accelerator that accelerates curing of the lightweight concrete compos ite. Another additive is a hardening agent that enhances hardening of the lightweight concrete composite. When used, the calcium chloride accelerator and the hardening agent are each added to the lightweight concrete composite in an amount equal to 2% of total weight of the cement To install the blocks 10 and thus build a retaining Structure in the form of a wall, enclosed area, raised garden, flower bed, and the like, any uneven ground must first be leveled. If necessary a Small trench may be dug to receive a bottom layer of the blocks 10. Leveling ground or digging a trench is unnecessary if the blocks 10 will reside on a level Surface Such as a concrete patio. The blocks 10 are light weight and thus easily carried. The blocks 10 are further easily cut with a Saw and in particular a chain Saw. Conse quently, the blocks 10 may be cut if necessary to a desired size and laid end to end to form a first layer. The ends the blocks 10 further may be Secured together using any Suitable adhesive or fastener. Additional blocks 10 may be cut if necessary to the desired size and laid end to end on top of the first layer to form a second layer. Not only may the ends of the additional blocks 10 be secured together using any Suitable adhesive or fastener, but also the additional blocks 10 forming the second layer may be secured to the blocks 10 forming the first layer using any Suitable adhesive or fas tener. Still further layers of blocks 10 may be stacked and

5 secured as described above until the desired height for the retaining structure is reached. The ends of the blocks 10 may be cut at any angle So that retaining Structures with different shapes may be constructed. Illustratively, three, four, five, and more sided retaining Structures may be built depending upon the angle of the cut along an end of a block 10. The blocks 10 are accordingly extremely advantageous for build ing retaining structures in the form of a walls, enclosed areas, raised gardens, flower beds, and the like because they are lightweight, easily cut and Stacked, and more impor tantly do not introduce harmful chemicals into the environ ment Although the present invention has been described in terms of the foregoing embodiment, Such description has been for exemplary purposes only and, as will be apparent to those of ordinary skill in the art, many alternatives, equivalents, and variations of varying degrees will fall within the Scope of the present invention. That Scope, accordingly, is not to be limited in any respect by the foregoing description; rather, it is defined only by the claims that follow. 1. A lightweight concrete composite block, comprising polystyrene, cement, water, and glass mixed to formulate a lightweight concrete composite, wherein the lightweight concrete composite is cured into the lightweight concrete composite block. 2. The lightweight concrete composite block according to claim 1, wherein the polystyrene is recycled polystyrene. 3. The lightweight concrete composite block according to claim 1, wherein the polystyrene is ground into particles having a diameter of less than of an inch. 4. The lightweight concrete composite block according to claim 1, wherein the glass is recycled glass. 5. The lightweight concrete composite block according to claim 1, wherein the glass is ground into particles having a diameter of less than /4 of an inch. 6. The lightweight concrete composite block according to claim 1, wherein the cement is Portland cement. 7. The lightweight concrete composite block according to claim 1, wherein the water comprises between 40% and 50% by total weight of the cement. 8. The lightweight concrete composite block according to claim 1, wherein the polystyrene comprises between 75% and 95% by total volume of the cement. 9. The lightweight concrete composite block according to claim 1, wherein the glass comprises between 40% and 45% by total weight of the cement. 10. The lightweight concrete composite block according to claim 1, wherein fly ash may be Substituted for a portion of the cement. 11. The lightweight concrete composite block according to claim 1, wherein fly ash may be Substituted for cement up to 20% by total weight of the cement. 12. The lightweight concrete composite block according to claim 1, further comprising a calcium chloride accelerator mixed with the polystyrene, cement, water, and glass to formulate a lightweight concrete composite cured into the lightweight concrete composite block. 13. The lightweight concrete composite block according to claim 12, wherein the calcium chloride accelerator com prises an amount equal to 2% of total weight of the cement. 14. The lightweight concrete composite block according to claim 1, further comprising a hardening agent mixed with the polystyrene, cement, water, and glass to formulate a lightweight concrete composite cured into the lightweight concrete composite block. 15. The lightweight concrete composite block according to claim 14, wherein the hardening agent comprises an amount equal to 2% of total weight of the cement. 16. The lightweight concrete composite block according to claim 1, wherein the lightweight concrete composite block comprises a horizontal axis greater than a vertical axis to facilitate Stacking thereof. 17. A method of manufacturing lightweight concrete composite blocks, comprising: mixing polystyrene, cement, water, and glass to formulate a lightweight concrete composite; and curing the lightweight concrete composite into light weight concrete composite blocks. 18. The method of manufacturing lightweight concrete grinding the polystyrene into particles prior to mixing the polystyrene with the cement, water, and glass to formulate the lightweight concrete composite. 19. The method of manufacturing lightweight concrete composite blocks according to claim 18, wherein the poly Styrene is ground into particles having a diameter of less than of an inch. 20. The method of manufacturing lightweight concrete grinding the glass into particles prior to mixing the glass with the polystyrene, cement, and water to formulate the lightweight concrete composite. 21. The method of manufacturing lightweight concrete composite blocks according to claim 20, wherein the glass is ground into particles having a diameter of less than /4 of an inch. 22. The method of manufacturing lightweight concrete composite blocks according to claim 17, wherein the water comprises between 40% and 50% by total weight of the cement. 23. The method of manufacturing lightweight concrete composite blocks according to claim 17, wherein the poly styrene comprises between 75% and 95% by total volume of the cement. 24. The method of manufacturing lightweight concrete composite blocks according to claim 17, wherein the glass comprises between 40% and 45% by total weight of the cement. 25. The method of manufacturing lightweight concrete composite blocks according to claim 17, wherein fly ash may be Substituted for a portion of the cement. 26. The method of manufacturing lightweight concrete composite blocks according to claim 17, wherein fly ash may be substituted for cement up to 20% by total weight of the cement. 27. The method of manufacturing lightweight concrete a calcium chloride accelerator mixed with the polystyrene, cement, water, and glass to formulate a lightweight concrete composite cured into the lightweight concrete composite blocks. 28. The method of manufacturing lightweight concrete composite blocks according to claim 27, wherein the cal cium chloride accelerator comprises an amount equal to 2% of total weight of the cement.

6 29. The method of manufacturing lightweight concrete a hardening agent mixed with the polystyrene, cement, water, and glass to formulate a lightweight concrete com posite cured into the lightweight concrete composite blocks. 30. The method of manufacturing lightweight concrete composite blocks according to claim 29, wherein the hard ening agent comprises an amount equal to 2% of total weight of the cement. 31. A method of installing lightweight concrete composite blocks to build a retaining Structure, comprising: providing lightweight concrete composite blocks, com prising polystyrene, cement, water, and glass mixed to formulate a lightweight concrete composite, wherein the lightweight concrete composite is cured into the lightweight concrete composite blocks, cutting a first lightweight concrete composite block to a desired length; placing the first lightweight concrete composite block at a desired location; cutting a Second lightweight concrete composite block to a desired length; placing the Second lightweight concrete composite block on the first lightweight concrete composite block, and Securing the Second lightweight concrete composite block with the first lightweight concrete composite block. 32. The method of installing lightweight concrete com posite blocks to build a retaining Structure according to claim 31, further comprising: cutting a third lightweight concrete composite block to a desired length; placing the third lightweight concrete composite block adjacent the first lightweight concrete composite block, and Securing the third lightweight concrete composite block with the first lightweight concrete composite block. 33. The method of installing lightweight concrete com posite blocks to build a retaining Structure according to claim 32, further comprising: cutting a fourth lightweight concrete composite block to a desired length; placing the fourth lightweight concrete composite block on the third lightweight concrete composite block and adjacent the Second lightweight concrete composite block, and Securing the fourth lightweight concrete composite block with the Second and third lightweight concrete com posite blocks.