Pavement Crack Treatment

Similar documents
Asphaltic Concrete Pavements Crack Treatments. A Pavement Preservation Process. Why Crack Treatment? Crack Treatments Overview and Objective

Pavement Preservation with Crack Treatments. Tom Kelly

Understanding Crack Sealing Materials and Specification Requirements

"Crack Sealing Best Practices"

CRACK SEALING AND FILLING TREATMENTS FOR ASPHALT CONCRETE PAVEMENTS. Jim Chehovits Vice President Operations Crafco, Inc August 27-30, 2012

Maintenance & Rehabilitation. Treatments. Crack Sealing. Sealant Types. Asphalt Pavement Preservation: Identification of Alternative Treatments

Crack Sealing Innovations

Arizona AGC Pavement Preservation Series Crack Sealing and Crack Filling Guide - Application and Construction

Crack Sealing New York State. Guy Hildreth NYSDOT Materials Bureau Albany, NY

Pavement Maintenance Best Practices. Thomas J. Wood

Session 10: Joint Resealing and Crack Sealing 10.1

LRRB 822 Project 822: Recommended Practices for Crack Sealing HMA Pavement

HAWAII DEPARTMENT OF TRANSPORATION HIGHWAYS DIVISION PAVEMENT PREVENTIVE MAINTENANCE GUIDELINES JUNE 2003

Section 502. HMA CRACK TREATMENT

Mastic Application Method Statement

Recommended Practices for Crack Sealing HMA Pavement

Alligator Cracking. Light. Medium. High

Asphalt Pavement Maintenance and Rehabilitation Strategies

(Flexible Pavements) From Maintenance Technical

Prevention of Transverse Bumps Over Crack Sealant During Asphalt Overlay Construction

550 Surface Treatments

37th Annual Rocky Mountain Asphalt Paving Conference February 25, 2010 Greg Milburn

Liquid Road Bituminous Surface Treatment for Parking Lots

MICRO-SURFACING - OPSS 336

Types of Joints in Concrete Pavements Why Seal Joints? Types of Sealants Proper Silicone Installation Inspection and Project Review Common Issues and

UNIQUE PAVING MATERIALS. Cleveland, Ohio. Started in 1959 Unique is the oldest continuous cold mix producer in the USA.

RMACES Tad McDonald February Joint Adhesive

Annual Costs Any costs associated with the annual maintenance and repair of the facility.

Tools and Tactics for Roadway Pavement Preservation: An Implementation Guide to Preserving High-Traffic-Volume Roadways

Choosing the Right Preservation Treatment for Flexible Pavements

Streets Evaluation Manual

CONCRETE Joint and Crack Sealing Basics

Protect Your Pavement Asset Like the Rest! Is Pavement on your Radar Screen? Parking Lots & Low Volume Facilities

INDEX DESCRIPTION MATERIALS EQUIPMENT CONSTRUCTION MEASUREMENT AND PAYMENT 8

CONSTRUCTION SPECIFICATION FOR CONCRETE PAVEMENT AND CONCRETE BASE

CONSTRUCTION SPECIFICATION FOR ROUTING AND SEALING CRACKS IN ASPHALT PAVEMENT

Pavement Distress Categories

Section 3 Specification 3.30 Asphalt Pavement Crack Routing and Sealing TABLE OF CONTENTS

Special Provision No. 341S01 April 2016

Q. Why crack seal? A. Preventive (intended to stop something undesirable from happening) Defensive, Precautionary, Deterrent, Protective.

Pavement Management 101 White Paper

PREVENTATIVE MAINTENANCE

Bump Formation & Prevention

FEDERAL AID ROAD CONDITION REPORT FOR BRANCH COUNTY 2018

Pavement Preservation ODOT Leading the Way

PAVEMENT MARKINGS. Presented by: Tom Clayton Director of Training and Member Services CAPA/RMAEC

Research. Saw and Seal Repair Chisholm / Hibbing Airport Taxiway Final Report

Estimated Cost per SY Crack Seal (CR) $ No Change Fog Seal (FS) $ No Change

Caltrans Maintenance Technical Advisory Guide (MTAG)

JUNTOPLAST C 1. DESCRIPTION 2. SPECIFICATIONS 3. PROPERTIES

STRUCTURAL EVALUATION & TREATMENT SELECTION FOR LOCAL ROADS. Nick Jones Local Technical Assistance Program Utah State University

SURFACE DISTRESS SURVEYS

ROAD CONDITION REPORT KALAMAZOO COUNTY MAY Prepared by the Kalamazoo Area Transportation Study (269)

Introduction to Pavement Overlays

Strawser Construction Inc.

Asphalt Pavement Forensics: Understanding the Problem to Better Determine the Solution

CONSTRUCTION SPECIFICATION FOR COLD IN-PLACE RECYCLED MIX

Bituminous mix design

BOCA Project Suitability, Design and Construction

Polymer Concrete Patching Materials. Todd Donmyer P.E. Area Engineer District 61

Methods for Maintenance of flexible Asphalt Pavements and Preventative life time

2010 Midwestern Pavement Preservation Partnership Conference

MANUFACTURERS OF PAVEMENT PRESERVATION PRODUCTS SINCE. Presented by Jeremiah Stratton

Andrew Hipolit, PE, PP, CME. What s New in Paving? 14 th Annual Public Works Continuing Education Conference

KANSAS DEPARTMENT OF TRANSPORTATION SPECIAL PROVISION TO THE STANDARD SPECIFICATIONS, EDITION OF 1990

Marathon Sealing FZE Company Portfolio

Asphalt Rubber Producers Group SP~ALTRUBBERPROWCERSGROUP 3336 NORTH 32ND STREET, SUITE 106 PHOENIX, ARIZONA (602)

THINLAY ASPHALT FOR PAVEMENT PRESERVATION

The Right Treatment for Resurfacing Projects. Clark Morrison, PE February 7, 2017

Marathon Sealing FZE Company Portfolio

Concrete Pavement Preservation:

KANSAS DEPARTMENT OF TRANSPORTATION SPECIAL PROVISION TO THE STANDARD SPECIFICATIONS, 1990 EDITION

ROAD CONDITION REPORT KALAMAZOO COUNTY

THIN ASPHALT OVERLAYS FOR PAVEMENT PRESERVATION

Polyurea stands out as a joint filler.

THIN ASPHALT OVERLAYS FOR PAVEMENT PRESERVATION

Manual of Practice. Materials and Procedures for Sealing and Filling Cracks in Asphalt-Surfaced Pavements. FHWA Report No.

PREVENTATIVE MAINTENANCE OF ASPHALT CONCRETE PAVEMENTS

53.5 ASPHALT PAVEMENT CRACK ROUTING AND SEALING

Technology Transfer Program

TABLE OF CONTENTS. Contents. Tables. Federal Aid Condition Maps

HMA Base Repair RPR Spring Meeting February 23, 2017 Ken Walschlager

Report Number: CP2C

PMIS Treatment Selection Questionnaire

PARKING LOT SEALANT. For additional information contact your Authorized Crafco Representative Product Data Sheets

GlasGrid Asphalt Pavement Reinforcement. October 21, 2016

Pavement Preservation with Thin Lift Concrete Overlays. Dale Harrington, P.E. Representing the National Concrete Pavement Technology Center

Field Guide. Asphalt Pavement Maintenance T 2 CENTER FOR TRANSPORTATION STUDIES. Field Guide MANUAL NUMBER REV MINNESOTA DEPARTMENT

Concrete Overlays... Northwest Pavement Management Association 2011Conference Jim Powell, P.E.

Best practices for crack treatments in asphalt pavements

KU Design Guidelines APPENDIX II PERMEABLE BITUMINOUS PAVEMENT

CHAPTER 2 ASPHALT CONCRETE MIXTURES

Széchenyi István University Faculty of Architecture, Civil Engineering and Transport Sciences Department of Transport Infrastructure.

BONDED CONCRETE OVERLAY ON ASPHALT

BONDED CONCRETEE OVERLAY OF ASPHALT PAVEMENTS MECHANISTIC-EMPIRICAL DESIGN GUIDE (BCOA-ME):

A STUDY OF POURED JOINT SEAL MATERIALS. D. L. O'Connor Supervising Chemical Engineer

The California Asphalt Pavement Association. February 2, 2017 WRAPP Pavement Preservation Workshop Doubletree Ontario Airport, Ontario, CA

Rehabilitation Strategies for Bonded Concrete Overlays of Asphalt Pavements

21 PAVEMENTS General Administrative Requirements Standards Personnel Certification

SPECIAL SPECIFICATION 4897 Repair Structural Concrete

Transcription:

Pavement Crack Treatment Crack treatment overview. Why and when to treat cracks. Evaluating pavement and selecting product. Proper application and equipment.

Pavement Crack Treatment Crack treatment overview. Why and when to treat cracks. Evaluating pavement and selecting product. Proper application and equipment.

Why treat cracks? Prevents water intrusion into the sub-base.

Why treat cracks? Prevents incompressible intrusion. Improves ride quality smoothness.

Why treat cracks? Slows down pavement deterioration.

Why treat cracks? Cracks are inevitable, and neglect leads to accelerated cracking and potholing, further reducing pavement serviceability. (FHWA-RD-99-147)

Why treat cracks? With proper and timely application, crack sealing and filling can extend pavement life past the point where the cost-benefit of added pavement life exceeds the cost of conducting the operation. (FHWA-RD-99-147)

Why treat cracks? Protect your largest investment. Pavement failure imminent Crack treatments are costeffective, up to 9 years of performance. Extends pavement life.

When to Seal Cracks? Soon after they appear any crack opening will allow moisture penetration into pavement foundation (subbase). At minimum all cracks 1/8.

What cracks to treat? Water Intrusion Incompressible Intrusion Edge Joints

Pavement Crack Treatment Crack treatment overview. Why and when to treat cracks. Evaluating pavement and selecting product. Proper application and equipment.

Crack Evaluation Working (high movement) 3mm movement -Thermal Non-working (low or no movement) < 3mm movement -Longitudinal -Block -Fatigue

Two Different Treatments Crack Sealing Working cracks - [10% of cracks]- The placement of specialized treatment materials above or into working cracks using unique configurations to prevent the intrusion of water and incompressibles into the crack. (FHWA-RD-99-147)

Crack Sealing Treatment Use: In thermal cracks. Routed reservoirs. Pavements in good condition- >20 transverse crack spacing, minor other cracking. Sealants that are flexible and extensible at lowest temperatures encountered.

Type of crack- thermal (transverse) Definition: Moving cracks formed by temperature related pavement/sub grade movement. Generally in transverse direction. (perpendicular to center line) Generally full width of street or road. Generally >20 foot spacing. Considered working cracks- 3mm movement. Will develop in 2-7 years on most new pavements, 1-3 years on overlaid concrete.

Crack Preparation / Routing Rout at least 1/8 from each crack face. Keep centered over crack. Reduce spalling by using as many cutters as possible.

Crack Preparation / Routing Rout size recommendation Standard Reservoirand-Flush Standard Recessed Band-Aid Shallow Recessed Band-Aid

Two Different Treatments Performance Crack Filling Non-working cracks - [90% of cracks]- The placement of ordinary treatment materials into non-working cracks to substantially reduce infiltration of water and to reinforce the adjacent pavement. (FHWA-RD-99-147)

Crack Filling Treatment Use: In longitudinal, block, fatigue and closely spaced transverse cracks (< 20 spacing). In wheel paths and high traffic areas. Stiffer more traffic resistant product. Routed or non-routed reservoirs (use discretion), over-band application. Pavements in fair to poor condition.

Crack Type Longitudinal Definition: Can develop in 2-5 years along with thermal cracks. Occur in longitudinal (parallel to center line) direction. Caused by thermal movement, construction joints and edge joints. Considered low movement, nonworking cracks- < 3mm movement.

Crack Type - Fatigue (alligator) Definition: Caused by repeated traffic loading Occurs in heavy traffic areas and wheel paths. Cracks form in closely spaced, interconnecting block patterns. Sure sign of pavement structural failure. Considered low or no movement nonworking cracks- < 3mm movement.

Crack Type - Fatigue (alligator) Same street- slurry seal treatment two years later.

Slurry Seal Slurry Seal Industry: Crack sealing is absolutely necessary for optimum slurry seal performance. All cracks 1/8 and larger. Can slurry seal over fresh hot-pour crack sealant the next day when necessary. Preferably, when time permits, wait 2-3 months before slurry sealing over crack sealant.

Large Cracks Polymer modified/aggregate materials No Air Voids No Compaction Adhesive

Forget It!

Product Selection Cohesive Failure Adhesive Failure

Product Selection Crack sealants and crack fillers need to remain functional over the range of anticipated pavement temperatures. Determine temperature ranges with LTPPBind www.tfhrc.gov/pavement/ltpp/reports/03080/ www.tfhrc.gov/pavement/ltpp/ppt/bind.ppt www.fhwa.dot.gov/pavement/ltpp/bind/dwnload

Types of products: (FHWA-RD-99-147) Crack Filling Emulsion and asphalt cement fillers - At best 2 to 4 years performance in un-routed non-working cracks Rubber and fiber-modified asphalt fillers -6 to 8 years performance in unrouted non-working cracks

Types of products: (FHWA-RD-99-147) Crack Sealing Rubberized (polymermodified) asphalt sealants 5-9 years performance in routed working cracks Rubberized (polymermodified) asphalt sealants 2.5-5 years performance in un-routed working cracks

Pavement Crack Treatment Crack treatment overview. Why and when to treat cracks. Evaluating pavement and selecting product. Proper application and equipment.

Proper equipment - Basics

Proper equipment - Basics Melter Applicator Oil-jacketed Thermostatic heat controls Continuous agitation Over-heating safety controls Right size for operation Many commercial versions * Construction of HMA Pavements- Asphalt Institute

Proper equipment - Basics PAVEMENT CUTTER

Proper equipment - Basics Worn Cutters will not provide a good reservoir. New Cutter Worn Cutter

Installation Choices Rout or Not Size of Rout Cleaning Recess Flush Overband

Basic Needs Requirements All applications Clean- most important Dry Intact pavement Proper temperature (pavement 40 F and application 400 F)

Cleaning Methods Clean Crack Unclean Crack Compressed air - sufficient pressure and velocity Vacuum - in combination with compressed air Heat lance - used to warm pavement when needed Routing - cuts new bonding surface

Flush Fill Seal Clean Crack No Sealant on the pavement surface

Recommended Overband Correct

NOT Recommended

Summary (Why Crack Seal?) Prevents water intrusion into subbase Prevents incompressible intrusion Improves ride quality smoothness Slows down pavement deterioration Cost effective

Summary (What Crack Treatment?) Pavement evaluation Determine if Crack Sealing or Crack Filling treatment is needed Determine temperature (high/low extremes) Select product Proper application