MODIFIED MEMBRANE BASE SHEET MATERIAL SPECIFICATIONS: Tear Strength 2 in/min ASTM D 5147 110 lbf. MD 110 lbf. XD Tensile Strength 2 in/min ASTM D 5147 100 lbf. MD 100 lbf. XD Elongation ASTM D 5147 2.5%. Low Temp. Flex. ASTM D 5147-20 o F MODIFIED MEMBRANE ROOFING & FLASHING SURFACE PLY / MINERAL Tear Strength 2 in/min ASTM D 5147 310 lbf. MD 310 lbf. XD Tensile Strength 2 in/min ASTM D 5147 500 lbf. MD 500 lbf. XD Elongation ASTM D 5147 3.5% MD 3.5% XD. Thickness (min) ASTM D 5147 155 mils Recycled Content Pre Consumer = N.A. Post Consumer = 6% MODIFIED MEMBRANE ROOFING SURFACE PLY / SMOOTH Tear Strength 2 in/min ASTM D 5147 900 lbf. MD 950 lbf. XD Tensile Strength 2 in/min ASTM D 5147 500 lbf. MD 550 lbf. XD Elongation ASTM D 5147 6.0% MD 6.0% XD. Recycled Content Pre Consumer = N.A. Post Consumer = 7.57% 83
MODIFIED MEMBRANE ROOFING SURFACE PLY / MINERAL AT REPAIR AREAS Tear Strength 2 in/min ASTM D 5147 225 lbf. MD 225 lbf. XD Tensile Strength 2 in/min ASTM D 5147 900 lbf. MD 950 lbf. XD Elongation ASTM D 5147 4.7% MD 5.0% XD. Recycled Content Pre Consumer = N.A. Post Consumer = 8.0% MODIFIED COAL TAR ADHESIVE: Viscosity Stormer Viscometer 125-175 sec. Flash Point ASTM D93 105 o F Non-Volatile ASTM D4479 77% Weight per gallon Drying Time to touch 9.4 lbs/gal 4-6 hours Recycled Content Post Industrial 70% FLASHING BASE PLY Tear Strength 2 in/min ASTM D 5147 315 lbf. MD 315 lbf. XD Tensile Strength 2 in/min ASTM D 5147 550 lbf. MD 550 lbf. XD Elongation ASTM D 5147 5.0% MD 6.0% XD. Thickness (min) ASTM D 5147 60 mils Mass of Desaturated Polyester/ ASTM D 146-97 4.0 lbs / 100 S.F. Glass Mat Recycled Content Post Consumer = 31.20% 84
TYPE IV ASPHALT Softening Point ASTM D 36 210-225 F Penetration @ 77 F ASTM D 5 12 25 Flash Point ASTM D 92 Min. 500 F Ductility @ 77 F ASTM D 113 1.5 cm. min. % solubility in trichloroethylene ASTM 2042 99% REINFORCING FABRIC: Weight ASTM D146-78a 1.32 lb/100 S.F. Moisture based on net weight ASTM D146-78a None Average tensile strength at 70 o F, min. Wrap Threads ASTM D146-78a 75 lbf/in. Filling Threads ASTM D146-78a 75 lbf/in. Treatment of fabric Weight ASTM D579-83 18.75% Type PVC/Acrylic water based Cure Temperature 300 o F min. Color Varies ASPHALT ELASTOMER: Asbestos Content ASTM D276-87 None Viscosity @ 77 o F ASTM D2196-81 600,00-2,000,000 cp Density @ 77 o F ASTM D1475-85 8.1 lb/gal Solids by weight, min. ASTM D412-87 62% Tensile strength @ 77 o F @ 100% elongation ASTM D412-87 40-100 psi Elongation, min. @77 o F ASTM D412-87 1,000% @ -30 o F ASTM D412-87 100% Recovery from elongation, min ASTM D412-87 90% Moisture Vapor Transmission Rate ASTM E398-83 0.50-1.10 g/100 in 2 /24 hrs 85
ASPHALT ELASTOMER: (con t) Resistance to sag, max. ASTM D4586-86 1/4 in FIBRATED ASPHALT MASTIC: Asbestos Content ASTM D276-87 None Viscosity @ 77 o F ASTM D2196-81 480,000-1,000,000 cp Density @ 77 o F ASTM D1475-85 9.3 lb/gal Solids by weight, min. ASTM D4586-86 80% Resistance to sag, max. ASTM D4586-86 1/8 in. Moisture Vapor Transmission Rate ASTM E398-83 0.10-0.40 g/100 in 2 /24 hrs @ 0.020 in. thickness GENERAL PURPOSE SEALANT: Adhesion-in-peel FS TT-S-00230C 25 lbs/in Tensile Strength ASTM D412-80 180 psi Ultimate Elongation ASTM D412-80 550% Weep & Sag FS TT-S-00230C Passes Staining FS TT-S-00230C Passes Weight-loss, cracking & chalking after heat aging FS TT-S-00230C Passes Hardness @ 77 o F, 50% RH (Shore A) FS TT-S-00230C 25 +/- 5 Durability FS TT-S-00230C Passes (on mortar) (Bond & Cohesion) granite and anodized aluminum at +/- 25% movement 86
PRIMER: Viscosity @ 77 o F (Ford cup B1) ASTM D1200-82 14.5 s Solids by weight ASTM D1644-75 44% Density ASTM D1475-85 7.8 lb/gal Flash point ASTM D3278-82 100 o F min. ASPHALTIC TAPE: Thickness 65 mils Tensile Strength ASTM D-412 750 lbs / in 2 Elongation ASTM D-412 170% Tear Strength ASTM D-412 165 ppi Low Temp. Flex. 37-GP-56M Pass Water Absorption 37-GP-56M <.1% 87